Lithium based batteries, whether they are solid-state batteries or traditional lithium-ion batteries, have similar structures. There are two electrodes (positive and negative) with a separator in between. During charging, ions migrate from the positive electrode (cathode) to the negative electrode (anode), and during discharging, ions migrate back again. Due to the impermeability of the membrane to electrons, electrons will pass through the connected load (such as a lamp) and cause it to light up (especially for more information on solid-state battery construction, please refer to here).
This description can be used to explain why current flows in the load, but it is not sufficient to understand where the energy comes from. Therefore, it is necessary to conduct more in-depth research on the functions of batteries.
Battery voltage window
Firstly, it is necessary to clarify why the voltage between the positive and negative electrodes can be measured. The voltage window of lithium based batteries is defined by partial reactions at the negative and positive electrodes, and correspondingly depends on the reactions occurring there. The measurable voltage at the two poles of a battery is the difference in voltage generated by each electrode:
UOC=U-negative pole - U-positive pole
The voltage of the negative and positive electrodes is not a fixed value, but depends on the charging state of the battery. However, fixed values for electrodes are often provided in literature (e.g. LCO of 3.9 V). These usually correspond to the average voltage.
The figure shows how to derive the final battery voltage from the negative and positive electrode potentials (displayed on the example battery LCO | graphite). The x-axis displays the amount of lithium proportionally bound in the electrode. For an (ideal) full battery x=1, for an empty battery x=0.

The measurable voltage at the positive and negative terminals of a battery is generated by the chemical reaction between lithium and the electrode. The following will provide a more detailed explanation using LCO (lithium cobalt oxide) positive electrode as an example. Figure 2 shows the discharge process of LCO | graphite battery. This is a lithium-ion battery with liquid electrolyte. In principle, this design is also applicable to solid-state batteries, although LCO and pure graphite as electrode materials are atypical and use further developed materials (such as silicon graphite as the negative electrode and NMC811 as the positive electrode).

Voltage is generated by the lithium ion charging and discharging process of the negative and positive electrodes. The reaction shown in the figure is also applicable to solid-state batteries, but the materials selected here are not typical and are for reference only.
During the discharge process, lithium ions migrate from the negative electrode to the positive electrode. LCO is a positive electrode with a layered structure. During the discharge process, lithium intercalates between the cobalt oxide layers. The reaction equation between lithium and cobalt oxide is as follows:
CoO2 + e– + Li+ → LiCoO2
The generation of externally measurable voltage is due to the intercalation reaction of lithium in each layer of layered oxide and the energy released during this exothermic process. With the help of the so-called Nernst equation, the voltage of a half cell can be calculated based on the concentration of substances in the battery:
Ured = U(0,red) – (RT / (ze F)) * ln(αRed / αOx)
U0,red: Electrode potential (can be read from the electrochemical voltage series table)
R: Universal gas constant
T: Temperature (Kelvin)
ze: Number of transferred electrons: Number of transferred electrons (lithium has only one valence electron, so here it is 1)
F: Faraday constant
αRed , αOx: Concentration of various redox reactants
The concentration of redox reactants varies with the change of electrode charge state. Therefore, the generated electrode voltage is essentially dependent on the electrode potential, which is calibrated based on temperature and charge state. It should be pointed out that some secondary reactions also occur in the battery, which also affects the generated voltage, so the above equation can only be used as a first approximation.
Due to the strong dependence of the Nernst equation on electrode potential, we attempt to select the element with the highest electrode potential here. The elements on the right side of the periodic table have reached a higher proportion here because the ionic radius of the elements has decreased, and electrons are more strongly attracted to the atomic nucleus. A stronger nuclear force will lead to a higher electrode potential.
This connection also explains why LCO (LixCoO2) and NMC811 are used as positive electrode materials. Among transition metals, these are the compounds with the highest half cell voltage.

Limitations of voltage window
The allowable voltage range of a battery is not only influenced by the electrodes, but also limited by the electrochemical window of the electrolyte used. Especially liquid electrolytes cannot withstand voltages exceeding 4.5V, as parasitic reactions occur between the positive electrode and the electrolyte, leading to slow decomposition of the electrolyte. Solid state batteries may be able to overcome this limitation in the medium term. For example, oxide electrolytes have a particularly wide voltage window, while sulfide electrolytes may also be able to withstand higher voltages with the addition of additional protective layers.
The second important limitation of the voltage window is that it is usually not possible to utilize the complete physical voltage window of the battery. For LCO cathodes, it is impossible to dissolve lithium from the cobalt layer by more than 70%, as this weakens the mechanical structure of the cathode and leads to accelerated aging. Therefore, compared to Li/Li+, the voltage of LCO batteries is limited to 4.2V. In terms of the negative electrode, it is usually not possible to remove all lithium ions, so some lithium ions still remain in the negative electrode, thereby reducing the maximum achievable capacity.
Determination of battery capacity
In order to provide maximum capacity for the battery, the negative and positive electrodes must be adjusted properly so that during the charging process, all lithium ions coming out of the positive electrode can find a storage location in the negative electrode structure. The ratio between the size of the negative electrode and the size of the positive electrode is called the N/P ratio, where N describes the mass fraction of the negative electrode and P describes the mass fraction of the positive electrode. Due to the fact that each lithium ion coming out of the positive electrode must find a position at the negative electrode, the size ratio N/P ≈ 1. However, it is difficult for lithium ions to always find a position at the negative electrode. During fast charging, lithium ions tend to deposit on the negative electrode (lithium plating) because they cannot quickly find vacant positions in the negative electrode structure. Due to lithium plating being one of the main damage mechanisms of batteries, the proportion of negative electrodes is slightly increased (N/P ≈ 1.04-1.2), so that ions do not have to search for idle positions for too long.

The capacity of various active materials is usually given in Ah/kg and can be calculated. The calculation only considers active materials. Chemical additives, contact surfaces, protective layers, etc. are ignored in the calculation of electrode theoretical capacity. When calculating, first determine the mass of the electrode material (in kg/mol). This value can be calculated by molar mass or obtained from a lookup table. For LCO, the molar mass is 0.09788 kg/mol. In the second step, the Avogadro constant can be used to calculate how many molecules are present in one kilogram of electrode material (for LCO, this is 6.15 * 10 ^ 24 atoms per kilogram).
As an alkali metal (element of the first main group), lithium only has one electron that can participate in chemical reactions. Each electron carries a negative fundamental charge e. Therefore, a lithium atom can release a fundamental charge e -.
In order to calculate capacity, it is now necessary to consider that during the discharge process, each lithium ion will transfer an electron through the connected load. Therefore, capacity is the product of the amount of charge carried by an atom and the number of atoms. For LCO, this results in a capacity of 274 Ah/kg. The capacity of other positive and negative electrode materials can also be calculated using the same method.
The calculated value represents the theoretically achievable energy density, but it is usually not very close to the actual value. For example, for LCO, only a portion of lithium can be removed during the charging process, so the theoretical capacity is not fully utilized, and the values obtained in practice are significantly lower. Nevertheless, the calculated data provides a good indicator for comparing different active materials.
Conclusion
The answer to the question of where the energy of lithium batteries actually comes from is clear: the reason is the redox reactions that occur more or less reversibly in the battery during charging and discharging. Due to the structure of the battery, electrons are forced to migrate to the negative electrode through the charger during charging. The resulting charge transfer causes lithium ions to also migrate to the negative electrode. During discharge, the process is reversed, with current flowing through the connected load and transmitting power. The voltage generated by a battery in a given state of charge can be calculated using the Nernst equation and mainly depends on the concentration of lithium ions on the electrodes. The more lithium ions migrate to the positive electrode side, the higher their concentration at the positive electrode, and the corresponding decrease in battery voltage.
The amount of energy that a battery can provide depends on its capacity. Capacity is a material specific variable that can be directly calculated from material data using simple equations.
All calculated parameters represent theoretical (maximum) values, which have not been achieved in practice. The voltage is limited by the electrolyte, and the full utilization of capacity will affect the mechanical stability of the positive electrode. In addition, to prevent parasitic deposition of lithium, slightly more negative electrode materials are always used than absolutely necessary. The goal of a good design process is to balance all these impacts to obtain practical batteries that can withstand hundreds of cycles in automotive use. The best battery is always the result of compromise.